Metal recovery is the ratio of weight of weld metal deposited to the weight of core wire melted. For Prima 7018 (AWS: E7018) metal recovery is 115% min.

In cheaper electrode, usually welder faces a problem of arc striking or knocking of electrode before use, where as in Prima 6013 (AWS: E6013) can operate even with 50 OCV (Open Circuit Voltage) that is a special characteristic of "Touch & Start welding" without any hassle.

As per AWS standard Prima 7018 (AWS: E7018) fulfills H5 level of hydrogen that is hydrogen content less than 5 ml per 100 gms of weld metal. CVN Impact strength of Prima 7018 (AWS: E7018) is 80 Joules at -20° C.

Prima HT Alloy 103 is the most recommended electrode for above application.

It is the measure of Ferrite phase present in Austenitic stainless steel. Presence of ferrite also compensate drawbacks of sulphur, phosphorus & other impurities in stainless steel. Application where corrosion resistant is of primary importance, ferrite number should be minimum.